Specific Process Knowledge/Etch/DRIE-Pegasus/nanoetch
Recipe | nano1.0 | nano1.1 | nano1.2 | nano1.3 |
---|---|---|---|---|
Tool | Pegasus | Pegasus | Pegasus | Pegasus |
C4F8 (sccm) | 52 | 52 | 52 | 52 |
SF6 (sccm) | 38 | 38 | 38 | 38 |
O2 (sccm) | 0 | 0 | 0 | 0 |
Coil power (W) | 800 (forward) | 600 (forward) | 800 (forward) | 600 (forward) |
Platen power (W) | 50 | 50 | 50 | 40 |
Pressure (mtorr) | 4 | 4 | 4 | 4 |
Process time (s) | 120 | 120 | 120 | 120 |
Nominal line width | Etched depths (nm) | |||
30 nm | ||||
60 nm | ||||
90 nm | ||||
120 nm | ||||
150 nm | ||||
Nominal line width | Etch rates in trenches (nm/min) | |||
30 nm | ||||
60 nm | ||||
90 nm | ||||
120 nm | ||||
150 nm | ||||
Etch rates in zep resist (nm/min) | ||||
One point on wafer | ||||
Images | Images | Images | Images | Images |
The nanoetch