Revision as of 16:17, 24 March 2011 by Jml (talk | contribs) (Etching of nanostructures in Si using DRIE-Pegasus: nano1.1 recipe, Run ID 1815, time 120 secs, SF6 38, C4F8 52, 4mtorr, 600/50 coil/platen, 10 degs.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 96 KB, MIME type: image/jpeg)

Etching of nanostructures in Si using DRIE-Pegasus: nano1.1 recipe, Run ID 1815, time 120 secs, SF6 38, C4F8 52, 4mtorr, 600/50 coil/platen, 10 degs.