File:WF 2C3feb2011-150.jpg
Appearance
Size of this preview: 800 × 600 pixels. Other resolution: 1,024 × 768 pixels.
Original file (1,024 × 768 pixels, file size: 157 KB, MIME type: image/jpeg)
Etching of nanostructures in Si using DRIE-Pegasus: nano1.0 recipe, Run ID 1801, time 120 secs, SF6 38, C4F8 52, 4mtorr, 800/50 coil/platen, 10 degs.