Specific Process Knowledge/Thin film deposition/Deposition of Scandium Nitride
Appearance
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
Deposition of Scandium Nitride
Deposition of ScN can only be done by reactive sputtering using Sc target.
The only tool for this application is the Cluster-based multi-chamber high vacuum sputtering deposition system, commonly referred to as the 'Cluster Lesker.' The operating process is thoroughly documented and described in detail.:
- Deposition of Scandium Nitride (ScN) using reactive sputtering in Sputter-System Metal-Nitride(PC3) Source 1 (4-inch target)
At the moment (October 2023) we have a 4-inch Sc target (0.250" thick bonded to Cu) for PC3 Src1.