Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Scandium Nitride

From LabAdviser
Revision as of 11:44, 9 November 2023 by Eves (talk | contribs) (Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Scandium_Nitride&action=submit click here]''' <i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> == Deposition of Niobium Titanium Nitride == Deposition of ScN can only be done by reactive sputtering using Sc target. The on...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Feedback to this page: click here

Unless otherwise stated, this page is written by DTU Nanolab internal

Deposition of Niobium Titanium Nitride

Deposition of ScN can only be done by reactive sputtering using Sc target.

The only tool for this application is the Cluster-based multi-chamber high vacuum sputtering deposition system, commonly referred to as the 'Cluster Lesker.' The operating process is thoroughly documented and described in detail.:

At the moment (October 2023) we have a 4-inch Sc target (0.250" thick bonded to Cu) for PC3 Src1.