Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/SiO2 Etch/Cr mask
Appearance
Feedback to this page: click here
Unless otherwise stated, all content in this section was done by Berit Herstrøm, DTU Nanolab
- EM tests with Cr mask on full wafer 6 min etch
- EM tests with Cr mask on wafer piece on Si carrier 6 min etch
- EM tests with Cr mask on full wafer 6 min etch
- EM tests with Cr mask on full wafer 6 min etch