Etching of nanostructures in Si using the ICP metal etcher: Sinano3.5 recipe, Run ID 438 and 440, time 120 secs, Cl2 15, BCl3 5, 2mtorr, 900/60 coil/platen, 20 degs.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 14:50, 15 March 2011 | 1,024 × 768 (84 KB) | Jml (talk | contribs) | Etching of nanostructures in Si using the ICP metal etcher: Sinano3.5 recipe, Run ID 438 and 440, time 120 secs, Cl2 15, BCl3 5, 2mtorr, 900/60 coil/platen, 20 degs. |