Revision as of 14:49, 15 March 2011 by Jml (talk | contribs) (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.4 recipe, Run ID 431, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/90 coil/platen, 20 degs.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 99 KB, MIME type: image/jpeg)

Etching of nanostructures in Si using the ICP metal etcher: Sinano3.4 recipe, Run ID 431, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/90 coil/platen, 20 degs.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current14:49, 15 March 2011Thumbnail for version as of 14:49, 15 March 20111,024 × 768 (99 KB)Jml (talk | contribs)Etching of nanostructures in Si using the ICP metal etcher: Sinano3.4 recipe, Run ID 431, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/90 coil/platen, 20 degs.