Revision as of 14:41, 15 March 2011 by Jml (talk | contribs) (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.0 recipe, Run ID 417 and 418 and 419, time 150 secs, BCl3 5, HBr 15, 2mtorr, 900/50 coil/platen, 20 degs.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 768 pixels, file size: 102 KB, MIME type: image/jpeg)

Etching of nanostructures in Si using the ICP metal etcher: Sinano3.0 recipe, Run ID 417 and 418 and 419, time 150 secs, BCl3 5, HBr 15, 2mtorr, 900/50 coil/platen, 20 degs.