The injection molding machine is located in the basement of building 346 (room 904). The machine can be booked from LabManager (not active yet).


The following polymers are presently available:

Polystyrene Basell Lupolen

Topas (COC from Ticona) 5013S-04 6015S-04 6017S-04 8007S-04

Other polymers (PE, PBT, PCT, PC, POM, PP, PU, SAN) are available in smaller amounts. Ask Danchip for details (choi@danchip.dtu.dk).