Nickel deposition

Nickel can be deposited by e-beam evaporation or sputtering at DTU Nanolab. For electroplating you will have to contact other institutes at DTU, e.g., DTU Mechanical Engineering.

Some process information is available here for e-beam evaporated films:

In the chart below you can compare the different deposition equipment:

E-beam evaporation (Temescal) E-beam evaporation (Wordentec) Sputter deposition (Lesker) Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3))
General description E-beam deposition of Nickel E-beam deposition of Nickel Sputter deposition of Nickel Sputter deposition of Nickel
Pre-clean Ar ion bombardment RF Ar clean RF Ar clean
Layer thickness 10 Å to 1 µm * 10 Å to 1 µm * 10 Å to 5000 Å ** 10 Å to 5000 Å **
Deposition rate 2-10 Å/s 10-15 Å/s Depends on process parameters, about 1 Å/s Depends on process parameters, at least ~ 4 Å/s, see conditions here
Batch size
  • Up to 4x6" wafers
  • Up to 3x8" wafers (ask for holder)
  • Many smaller pieces
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
  • Pieces or
  • 1x4" wafer or
  • 1x6" wafer
  • Up to 10x4" or 6" wafers
  • Many smaller pieces
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon nitride
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Almost any that do not outgas.
  • Almost any that do not outgas. Check the cross-contamination sheet in Labmanager.
Comment
  • May use high-strength magnet for deposition.
  • May use high-strength magnet for deposition

* To deposit a cumulative thickness above 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine


** To deposit a cumulative thickness above 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine

Quality control of e-beam evaporated Ni films

Quality control (QC) for Wordentec
QC Recipe: Process 5
Deposition rate 10 Å/s
Thickness 100 nm
Pressure Below 4*10-6 mbar
QC limits Wordentec
Measured average thickness (Å) ± 10 %
Lowest accepted deposition rate (Å/s) 6 Å/s

Thickness is measured in 5 points with a stylus profiler.


Quality control (QC) for the Temescal
QC Recipe: Standard recipes/Ni
Deposition rate 10 Å/s
Thickness 100 nm
Pressure Below 1*10-6 mbar
QC limits Temescal
Deposition rate deviation ± 20 %
Measured average thickness ± 10 %
Thickness deviation across a 4" wafer ± 5 %

Thickness is measured in 5 points with a stylus profiler.
Additionally we examine the newly deposited films for particles using the particle scanner (if available, otherwise we use the Jenatech microscope in darkfield mode) and we monitor the sheet resistance of the Ti/Au films.