Revision as of 09:07, 3 December 2010 by BGE (talk | contribs) (Borofloat etch with silicon mask made in the Lesker at 200dg. Resist mask from the pattering is on and has been heated to 180 degrees before etching in 40% HF for 15 min.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (2,560 × 1,920 pixels, file size: 148 KB, MIME type: image/jpeg)

Borofloat etch with silicon mask made in the Lesker at 200dg. Resist mask from the pattering is on and has been heated to 180 degrees before etching in 40% HF for 15 min.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current09:07, 3 December 2010Thumbnail for version as of 09:07, 3 December 20102,560 × 1,920 (148 KB)BGE (talk | contribs)Borofloat etch with silicon mask made in the Lesker at 200dg. Resist mask from the pattering is on and has been heated to 180 degrees before etching in 40% HF for 15 min.

Metadata