Specific Process Knowledge/Etch/Etching of Silicon
Appearance
Etch of silicon can be done by either wet etch or dry etch. The standard setups for this here at DANCHIP are:
Wet etches:
- KOH etch
- Wet PolySilicon etch
Dry etches:
- Dry etch using RIE1 or RIE2
- Dry etch using ASE
Comparison of KOH etch, wet PolySilicon etch, RIE etch and ASE etch for etching of Silicon
| KOH | PolySilicon etch | RIE | ASE | |
|---|---|---|---|---|
| What is it good for: |
|
|
|
|
| Possible masking materials: |
|
? |
|
|
| Etch rate | <40nm/min to >600nm/min | |||
| Size of substrate | 4" and 6" in our standard bath | 4" in our standard bath | 4" (or smaller with carrier) | 6" (when it is set up for 6") and 4" (or smaller if you have a carrier) |
| Process volume | 25 wafers at a time | 25 wafers at a time | One wafer at a time | One wafer at a time |