Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Palladium

From LabAdviser

Feedback to this page: click here


Palladium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment:


E-beam evaporation (Temescal) E-beam evaporation (Wordentec) Sputter deposition (Sputter-System (Lesker))
General description E-beam deposition of Pd E-beam deposition of Pd Sputter deposition of Pd
Pre-clean Ar ion source none RF Ar clean
Layer thickness 10 Å - 600 nm* 10 Å - 600 nm* 10 Å - 600 nm*
Deposition rate 0.5 Å/s to 10Å/s 2 Å/s to 10Å/s Up to 4.3 Å/s
Batch size
  • Up to 4x6" wafers
  • Up to 3x8" wafers (ask for holder)
  • smaller wafers and pieces
  • Up to 6x6" wafers (deposition on one wafer at the time)
  • Up to 6x4" wafers (deposition on one wafer at the time)
  • smaller wafers and pieces
  • 1x4" wafer or
  • 1x6" wafer or
  • several small samples
Allowed materials
Comment

* If depositing more than 600 nm, please write to metal@nanolab.dtu.dk well in advance to ensure that enough material is present.