Specific Process Knowledge/Etch/Etching of Chromium
Jump to navigation
Jump to search
Feedback to this page: click here
Etching of Chromium
Etching of chromium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Chromium Etch Methods
Cr wet etch | ICP metal | IBE (Ionfab300+) | |
---|---|---|---|
Generel description | Wet etch of Cr premixed (Chrome etch 18) | Dry plasma etch of Cr | Sputtering of Cr - pure physical etch |
Etch rate range |
|
|
|
Etch profile |
|
|
|
Substrate size |
|
|
Smaller pieces glued to carrier wafer
|
Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|
|