Specific Process Knowledge/Thin film deposition/Deposition of ITO
Appearance
Feedback to this page: click here
Deposition of ITO
ITO (indium tin oxide) can be deposited by sputtering here at DTU Nanolab. An ITO target is used and it may be sputtered either non-reactively in Ar or reactively in a mixture of Ar and O2.
- Deposition conditions and a few results for ITO deposited for the acceptance test of the Sputter-System Metal-Oxide(PC1)
Comparison of the methods for deposition of ITO
| Sputter-System(Lesker) | Sputter-System Metal-Oxide(PC1) | |
|---|---|---|
| Generel description |
|
|
| Stoichiometry |
|
|
| Film Thickness |
|
|
| Deposition rate |
|
|
| Step coverage |
|
|
| Process Temperature |
|
|
| Substrate size |
|
|
| Allowed materials |
|
|