Process information for the Raith eLINE Plus system
The system was installed in the cleanroom in May 2022. As we get more familiar with the tool this page will be populated with relevant process information.
Dose information
The eLINE tool operates with four different dose types; area dose [pC/cm2], curved element dose [pC/cm2], line dose [pC/cm] and dot dose [pC]. Notice that the last two first are dose per area, while the last two are dose per length and dose per dot, respectively.
Table of dose to clear on Si substrate:
| Dose [µC/cm2] | |||
|---|---|---|---|
| Acc. voltage | AR-P 6200.09 (180 nm) | PMMA 950k | AR-N 8200.xx |
| 10 kV | 30 | ||
| 20 kV | 70 | ||
| 30 kV | 100 | ||