DREM 0.2kW

DREM 0.2 kW v2
Recipe General Pressure Gases Generators Matching Tem- pera- ture Results
C4F8 SF6 Ar Coil Platen Coil Platen
Platen Stb S/E Dp Et Cyc Dp Et Dp Et Dp Et Dp Et Dp Et Dp Et Dp Et Dp Et Runs Keywords
U/D H/L D B M D B M D B M D B M D B M D B M D B M L T L T L T L T
DREM 0.2kW newMFC Clamp Substrate,Pump to base, home platen matching unit, barc1, stab 1