Revision as of 09:29, 5 February 2021 by Bghe (talk | contribs) (Created page with "<gallery caption="Recipe no. 10: C06445_02 coil_2500W, platen:300W, He/C4F8= 17.5, C4F8/H2=1, Pressure:8.8mTorr, C4F8:25.6sccm, He:448.7sccm, H2:25.6sccm, 3:56 min " perrow="8...")