File:Amor540 24Hours.png

From LabAdviser
Revision as of 11:38, 4 June 2020 by Paphol (talk | contribs) (LPCVD Poly furnace Recipe: Amor540, deposition time 24hours, film thickness 2um.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (930 × 443 pixels, file size: 335 KB, MIME type: image/png)

LPCVD Poly furnace Recipe: Amor540, deposition time 24hours, film thickness 2um.