Descum results
Plasma asher 1
Descum of AZ5214E resist on 50mm silicon wafer. Wafer was placed horisontally in chamber on a 100 mm carier wafer.
Note: Plasma asher was cold before use
Plasma asher 2Descum of AZ Mir 701 resist on 100mm silicon wafer. Five wafers were placed vertically in chamber. Experiment parameters
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||