DOE1_SIO2_RIE1_Selectivitet_70.jpg (712 × 522 pixels, file size: 41 KB, MIME type: image/jpeg)

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current10:06, 24 November 2008Thumbnail for version as of 10:06, 24 November 2008712 × 522 (41 KB)BGE (talk | contribs)DOE1 SIO2 on RIE1 by BGE. Done in 2007-2007. Written in 2008. CHF3%=70
10:04, 24 November 2008Thumbnail for version as of 10:04, 24 November 2008712 × 522 (41 KB)BGE (talk | contribs)