ASE
|
AOE
|
DRIE-Pegasi
|
ICP Metal etch
|
III-V RIE
|
III-V ICP
|
IBE-IBSD Ionfab300+
|
| Pegasus 1
|
Pegasus 2
|
| Purpose
|
Primary uses
|
Formerly the primary silicon etcher; now polymers, Silicon oxides and nitrides may also be etched. 5% metal on the surface is allowed.
|
Etching of silicon oxides or nitrides
|
Silicon etching
|
Standard recipes for etching of Al, Cr and Ti, now also etches of W, TiW and Mo
|
Etching of silicon oxide, resist, BCB, silicon nitride, InP, InGaAs and GaAs on III-V substrates
|
Etching of III-V materials such as GaN, InP/InGaAsP/InGaAs, AlGaAs, GaAs
|
Physical Etching of all materials
|
| Alternative/backup uses
|
Backup silicon etcher
|
|
Barc etch
|
Silicon etcher
|
|
|
|
| General description
|
Plasma source
|
Inductively coupled plasma chamber with two RF generators; the coil and platen generator
|
Inductively coupled plasma chamber with two RF generators; the coil and platen generator
|
Inductively coupled plasma chamber with two RF generators; the coil (with outer and inner coil) and platen generator
|
Inductively coupled plasma chamber with two RF generators; the coil and platen generator
|
Parallel plate capacitor setup with RF power between the two electrodes
|
Inductively coupled plasma chamber with two RF generators; the coil and platen generator
|
Ion beam etcher - sputter etches with argon ions
|
| Substrate cooling/temperature
|
The electrode is oil cooled. Also, Helium backside cooling: -10oC to 20oC
|
The electrode is oil cooled. Also, Helium backside cooling: -10oC to 60oC
|
The electrode is oil cooled. Also, Helium backside cooling: -20oC to 30oC
|
The electrode is oil cooled. Also, Helium backside cooling: -10oC to 50oC
|
The electrode is oil cooled: Fixed at 20oC
|
The electrode is oil cooled with a special chiller. Also, Helium backside cooling: 20oC to 180oC
|
The electrode is oil cooled with a special chiller. Also, Helium backside cooling: 5oC to 60?oC
|
| Clamping
|
Electrostatic clamping (semco electrode)
|
Electrostatic clamping (TDESC)
|
Electrostatic clamping (TDESC)
|
Electrostatic clamping (TDESC)
|
No clamping
|
Mechanical clamping (weighted clamp with ceramic fingers)
|
Mechanical clamping
|
| Gasses
|
| SF6
|
O2
|
C4F8
|
| Ar
|
CF4
|
CHF3
|
H2
|
He
|
|
|
|
| SF6
|
O2
|
C4F8
|
| Ar
|
CF4
|
H2
|
| BCl3
|
Cl2
|
HBr
|
|
|
| SF6
|
O2
|
CF4
|
| Ar
|
CH4
|
H2
|
| HBr
|
BCl3
|
Cl2
|
|
|
| RF generators
|
- Coil generator
- Platen generator
|
- Coil generator
- Platen generator
|
- Coil generator
- Platen generator
- Low frequency platen generator
|
- Coil generator
- Platen generator
|
|
- Coil generator
- Platen generator
|
- Coil generator on plama chamber
- 3 accelerator grids between plasma chamber and process chamber
|
| Substrate loading
|
Loading via dedicated two-slot carousel load lock
|
Loading via dedicated two-slot carousel load lock
|
Loading via dedicated two-slot carousel load lock or via atmospheric cassette loader
|
Loading via dedicated two-slot carousel load lock
|
Loading via dedicated two-slot carousel load lock
|
Manual loading directly into process chamber
|
Loading via dedicated two-slot carousel load lock
|
Automatic loading via load lock
|
| Options
|
- Bosch multiplexing
- Parameter ramping
|
|
- Bosch multiplexing
- Parameter ramping
- SOI option
- Claritas endpoint detection
|
- Bosch multiplexing
- Parameter ramping
- SOI option
- Optical endpoint detection
|
- Parameter ramping
- Optical endpoint detection
|
|
- Parameter ramping
- Bosch multiplexing
- Optical endpoint detection
- Laser endpoint detection
|
|
| Allowed materials
|
|
- Silicon
- Fused silica
- Sapphire
- SiC
- Resists
- Some polymers
- <5% metal on the suface (for 4")
|
- Silicon
- Fused silica
- Sapphire
- SiC
- Resists
- Al,(Cr) as masking materials
|
- Silicon
- Fused silica
- Sapphire
- SiC
- Resists
|
- Silicon
- Fused silica
- Sapphire
- SiC
- Al, Cr, Ti, W, Mo, Nb
- Resists
|
- Silicon
- Fused silica
- Sapphire
- SiC
- GaAs, GaN, InP, with epitaxial layers
- Resists (at low temperature processing)
|
- Silicon
- Fused silica
- Sapphire
- SiC
- GaAs, GaN, InP, with epitaxial layers
- Resists (at low temperature processing)
|
- Almost any material, see LabManager
|