Data processing guidelines in Avantage

Use one processing grid to hold all spectra to be fitted.
Each processing grid has a peak table that holds all the peaks for each level. Making depth profiles cannot be made across processing grids. Survey spectra must be kept in separate grids - if not the peak table of the survey spectrum will get mixed with the high resolution spectra.
Do not mix snapshot and scanned spectra in processing grid