Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1
Appearance
XPS analysis of ALD deposited layers
How to get the data used in the example below
The wiki does not allow uploading of *.zip data files so the zipped data file has been renamed to a *.xls file. Therefore, do the following:
- Download this File:Experiment 2.xls.
- Rename the file Experiment_2.zip to Experiment_2.zip
- Extract to a folder on a local drive (right click and select 'Extract all'). Avantage will not work on network drives.
- Double click on the Experiment 2.VGX file and Avantage should start.
How to fit data with multiple spectra and levels
- Use one processing grid to hold all spectra to be fitted.
- Each processing grid has a peak table that holds all the peaks for each level. Making depth profiles cannot be made across processing grids. Survey spectra must be kept in separate grids - if not the peak table of the survey spectrum will get mixed with the high resolution spectra.
- Do not mix snapshot and scanned spectra in processing grid