Specific Process Knowledge/Thin film deposition/Deposition of Tin
Appearance
Feedback to this page: click here
Tin deposition
Tin can be deposited by e-beam evaporation. It was evaporated in the Alcatel e-beam evaporator, which is being decommissioned, but has not yet been evaporated in the Physimeca or the Temescal, which we have now (August 2018)
| E-beam evaporation (Temescal) | |
|---|---|
| General description | E-beam deposition of Sn
(line-of-sight deposition) |
| Pre-clean | Ar ion clean |
| Layer thickness | 10Å to 1µm* |
| Deposition rate | 1Å/s to 10Å/s |
| Pre-clean | Ar ion bombardment |
| Batch size |
|
| Allowed materials |
|
| Comment | Tin has not yet been deposited in the Temescal to date (August 2018).
Please contact the Thin Film group if you would like us to develop the process. |
* For thicknesses above 600 nm permission is required.