Palladium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment:


E-beam evaporation (Temescal) E-beam evaporation (Physimeca)
General description E-beam deposition of Pd E-beam deposition of Pd
Pre-clean Ar ion source RF Ar clean
Layer thickness 10 Å - 1 µm* 10 Å to 200 nm
Deposition rate 0.5 Å/s to 10Å/s 2 Å/s to 10Å/s
Batch size
  • Up to 4x6" wafers
  • Up to 3x8" wafers (ask for holder)
  • smaller wafers and pieces
  • 1x 2" wafer or
  • 1x 4" wafers or
  • Several smaller pieces
Allowed materials
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
Comment

* If depositing more than 600 nm, please write to metal@danchip.dtu.dk well in advance to ensure that enough material is present.