Deposition of Cu
Copper can be deposited by e-beam evaporation, sputtering or electroplating. In the chart below you can compare the different deposition equipments.
| E-beam evaporation (Temescal) | Sputter deposition (Lesker) | Electroplating (Electroplating-Cu) | |
|---|---|---|---|
| General description | E-beam deposition of Cu | Sputter deposition of Cu | Electroplating of Cu |
| Pre-clean | Ar ion bombardment | RF Ar clean | None |
| Layer thickness | 10Å to 1µm* | 10Å to 1µm** | thickness window undefined yet |
| Deposition rate | 1Å/s to 10Å/s | ~1Å/s | |
| Batch size |
|
|
|
| Allowed materials |
|
|
Base Materials:
Seed metals:
|
| Comment | As of August 2018, Cu has not yet been deposited in this machine. Contact the Thin Film group to develop a process. | Sample must be compatible with plating bath. Seed metal layer required to run electroplating process. |
** To deposit layers thicker than 600 nm permission is required to ensure that there is enough metal (contact metal@danchip.dtu.dk)
* To deposit layers thicker than 200 nm permission is required to ensure that there is enough metal (contact metal@danchip.dtu.dk)
Studies of Cu deposition processes
Roughness of Cu layers - Roughness of Cu layers deposited with Alcatel