File:Cr 405W 004mbar.jpg

From LabAdviser
Revision as of 10:14, 13 August 2008 by Kn (talk | contribs) (AFM picture of Cr layer sputter deposited in Wordentec. Settings: 405W, 0.004mbar)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (795 × 628 pixels, file size: 97 KB, MIME type: image/jpeg)

AFM picture of Cr layer sputter deposited in Wordentec. Settings: 405W, 0.004mbar