File:Cr 150W 001mbar.jpg

From LabAdviser
Revision as of 10:43, 12 August 2008 by Kn (talk | contribs) (AFM picture of sputter deposited Cr layer. 150W and 0.001 mbar used.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (795 × 628 pixels, file size: 331 KB, MIME type: image/jpeg)

AFM picture of sputter deposited Cr layer. 150W and 0.001 mbar used.