Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of AZO

From LabAdviser

Feedback to this page: click here

THIS PAGE IS UNDER CONSTRUCTION

AZO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment.


Sputtering deposition (Lesker) Atomic layer deposition (ALD Picosun R200)
General description Sputter deposition of AZO Atomic layer deposition of AZO
Pre-clean RF Ar clean
Layer thickness 10Å to 5000Å*
Deposition rate 2Å/s to 15Å/s
Batch size
  • Up to 1x4" wafers
  • smaller pieces
  • Pieces or
  • 1x4" wafer or
  • 1x6" wafer
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Silicon
  • Silicon oxide
  • Silicon nitride
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Carbon
Comment

* For thicknesses above 200 nm permission is required.