| Parameter | Recipe name: no name yet (testing recipe) |
|---|---|
| Coil Power [W] | 1200 |
| Platen Power [W] | 200 |
| Platen temperature [oC] | 0 |
| BCl3 flow [sccm] | 60 |
| Cl2 flow [sccm] | 30 |
| Pressure [mTorr] | 4 |
Etch rates in different materials using the standard "Silicon oxide etch with resist mask"
| Material to be etched | Etch rate using the above parameters |
|---|---|
| Al2O3 |
|