Specific Process Knowledge/Characterization/XPS/Processing/Basics/3fitting
Appearance
Feedback to this page: click here
Fitting the oxygen O1s core level
There is a few choices to make on the fitting of the O1s level. The level is an s-orbital and thus gives rise to a peak that is symmetric so any non-symmetric appearance must be caused several states of oxygen. The question is then to which states of oxygen they should be attributed. Below are shown the spectra of levels 0 (surface), 11 and 20.
We can establish that
- The main peak remains at fixed binding energy, and
- There is a shoulder at higher binding energy