Process parameters
Recipe Step Temp. Time Pres. Hardware Gasses RF powers Observations
SF6 O2 C4F8 Ar CF4 H2 CH4 BCl3 Cl2 HBr Coil Platen Runs Keywords
isoslow1 A 20 - 90 ? 50 ? 0 0 0 0 0 0 0 0 0 400 3 1 NA
r A 20 - 28 LF+B100 30 37 0 0 0 0 0 0 0 0 0 100 1 NA