Date Substrate Information Process Information SEM Images
Wafer info Exposed area Conditioning Recipe Wafer ID
2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-1, 80 cycles or 14:40 minutes C03991.02

2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-1, 80 cycles or 14:40 minutes C03991.05

3/6-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-1, 80 cycles or 14:40 minutes C04047.02

3/6-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-1, 80 cycles or 14:40 minutes C04047.05