Recipe Step Temp. Deposition step Etch step Process observations
Time Pres. C4F8 SF6 O2 Coil Time Pres. C4F8 SF6 O2 Coil Platen HW Runs Key words
mediumiso1 - 20 NA NA NA NA NA NA NA 25 0 150 0 600 3 - 1 NA
-






Mediumiso
Recipe Step Temperature Time Pressure C4F8 SF6 O2 Ar Coil Platen Runs Key words
mediumiso1 - 20 NA 25 0 150 0 0 600 3 1 NA
-