40% HF 3µm/min
Beaker
Maske?
Beskrives en hel process.
Comparison of wet Silicon Oxide etch and dry etches (RIE and AOE) etch for etching of Silicon Oxide
|
Wet Silicon Oxide etch (BHF and SIO Etch (wetting agent))
|
RIE
|
AOE
|
General description
|
|
- Anisotropic etch: vertical sidewalls
|
- Anisotropic etch: vertical sidewalls, especially good for deep etch and high aspect ratio etch
|
Possible masking materials
|
- Photoresist
- Silicon nitride
|
- Photoresist
- (Poly)Silicon
- Aluminium
- Chromium (ONLY RIE2!)
- Other metals that covers less the 5% of the wafer area (ONLY RIE2!)
|
- Photoresist
- (Poly)Silicon
- Aluminium
|
Etch rate
|
- ~75 nm/min (Thermal oxide) in BHF
- ~90 nm/min (Thermal oxide) in SIO Etch
|
- Typically 40-120 nm/min can be increased or decreased by using other recipe parameters.
|
- Typically 200-600 nm/min can be increased or decreased by using other recipe parameters.
|
Batch size
|
|
|
|
Size of substrate
|
|
- 4" wafers or smaller pieces
|
- 6" or 4" depending on the setup (smaller pieces if you have a carrier wafer)
|
Allowed materials
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- Blue film
- Gold (Au) and Nickel (Ni) (but only in BHF2 (KOH)!)
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
- Aluminium
- Chromium (ONLY RIE2!)
- Other metals that covers less the 5% of the wafer area (ONLY RIE2!)
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
- Aluminium
|