Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
24/10-2014 4" DUV-BoxC wafer stepper mask (50 nm barc + 250 nm krf)/Si Si / 60+ % on die Pegasus/jmli 3 minute TDESC clean + 30 sec barc etch danchip/jml/nano/nanoboost/nboost04 100 cycles or 13 minutes S004436


HiRes images of S004436