Specific Process Knowledge/Etch/ICP Metal Etcher/silicon oxide/By BGHE
Appearance
THIS PAGE IS UNDER CONSTRUCTION
I tried with two different gas regimes: CF4 and C4F8. I only made a few tests with CF4 since I got a very bad selectivity to the resist mask and I dicided to go for the C4F8 instead.
C4F8
CF4
I stopped trying with CF4 because I got bad selectivty to the resist and decided to focus on the recipe with C4F8 instead.