Overview of the standard processes: Processes A, B, C, D and SOI
The instrument was accepted on the basis of the performance of 5 processes. Below is a general comparison - to find more detailed information, go the web page for each process
Process name | Type | Purpose | Conditions during original runs | Best usage | |||
---|---|---|---|---|---|---|---|
Feature | Mask material | Etch load | Comments | ||||
Process A | Bosch | Fast etch | 80 µm trench | Photo resist | 12-13 % on 6" wafer | ||
Process B | Bosch | Fast etch | 30 µm diameter via | Photo resist | 12-13 % on 6" wafer | ||
Process C | Continuous | Very slow etch | 50 nm posts | Aluminum | 99.9 % on 4" wafer | ||
Process D | Bosch | Smooth sidewall etch | 10 µm trench | Photo resist | 50 % on 6" wafer |