Specific Process Knowledge/Thin film deposition/PECVD/Doping
Appearance
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
Recipe
| Recipe name | SiH4 flow [sccm] | N2O flow [sccm] | N2 flow [sccm] | B2H6 flow [sccm] | Pressure [mTorr] | Power [W] | Description |
| 1PBSG | 17 | 1600 | 0 | 135 | 500 | 800LF | BPSG glass for drive in boron in Silcion |