Revision as of 17:04, 11 March 2015 by Hoal (talk | contribs) (ARGUS image of martensitic steel. Image is obtained using the following settings: Accelerating voltage: 15 kv Probe current: 3.9 nA ARGUS detector, 9 degrees tilted and 17 mm away from the sample)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 884 pixels, file size: 1.4 MB, MIME type: image/jpeg)

ARGUS image of martensitic steel. Image is obtained using the following settings: Accelerating voltage: 15 kv Probe current: 3.9 nA ARGUS detector, 9 degrees tilted and 17 mm away from the sample

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current17:04, 11 March 2015Thumbnail for version as of 17:04, 11 March 20151,024 × 884 (1.4 MB)Hoal (talk | contribs)ARGUS image of martensitic steel. Image is obtained using the following settings: Accelerating voltage: 15 kv Probe current: 3.9 nA ARGUS detector, 9 degrees tilted and 17 mm away from the sample

There are no pages that use this file.

Metadata