Revision as of 16:04, 17 February 2015 by Paphol (talk | contribs) (Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour. Result from Trine H. Christensen DTU Space)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,164 × 938 pixels, file size: 31 KB, MIME type: image/png)

Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour. Result from Trine H. Christensen DTU Space

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current16:04, 17 February 2015Thumbnail for version as of 16:04, 17 February 20151,164 × 938 (31 KB)Paphol (talk | contribs)Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour. Result from Trine H. Christensen DTU Space