Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
2/12-2014 4" Wafer with travka50 mask AZ standard Si / 50+ % Pegasus/jmli 10 minute TDESC clean danchip/jml/showerhead/prD/PrD01, 110 cyc or 6:14 mins S004691 New showerhead