Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/ProcessD/original

From LabAdviser
Revision as of 18:10, 18 December 2014 by Jmli (talk | contribs) (Created page with " {| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" |+ '''Process runs''' |- ! rowspan="2" width="40"| Date ! colspan="4" width="120"| Substrate Informat...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
20/11-2014 6" Wafer with 210 nm oxide and 1800 nm polysilicon standard stepper mask (50 nm barc + 320 nm krf) Si / 50+ % Pegasus/jmli 10 minute TDESC clean + 45 sec barc etch danchip/jml/showerhead/polySi etch DUV mask, 20 cycles or 3:02 minutes S004675 Old showerhead

1/12-2014 1/4 6" Wafer with 210 nm oxide and 1800 nm polysilicon crystalbonded on carrier standard stepper mask (50 nm barc + 320 nm krf) Si / 50+ % Pegasus/jmli 10 minute TDESC clean + 45 sec barc etch danchip/jml/showerhead/polySi etch DUV mask, 20 cycles or 3:02 minutes S004675 New showerhead