Comparison of continuous processes
Comparison of switched processes
Recipe | Step | Temp. | Deposition step | Etch step | Process observations | |||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Time | Pres. | C4F8 | SF6 | O2 | Coil | Time | Pres. | C4F8 | SF6 | O2 | Coil | Platen | Hardware]] | Runs | Key words | |||
- | ||||||||||||||||||
Baseline | - | 30 | 2.3 | 10 | 50 | 0 | 0 | 600 | 5.0 | 10 | 20 | 60 | 5 | 400 | 40 | - | 1 | |
base-B | - | 30 | 2.15 | 10 | 50 | 0 | 0 | 600 | 5.0 | 10 | 20 | 60 | 5 | 400 | 40 | - | 1 | |
base-C | - | 30 | 2.15 | 10 | 50 | 0 | 0 | 600 | 5.0 | 10 | 20 | 60 | 5 | 400 | 40 | - | 1 |