Drying Comparison Table
| Equipment
|
Spin dryer 1
|
Spin dryer 2
|
Spin dryer 3
|
Spin dryer 4
|
Critical point dryer
|
Ethanol fume dryer
|
N2 guns
|
| Location
|
|
|
|
|
|
|
|
- In fumehoods and at chemical benches
|
| Purpose
|
|
|
|
|
|
- Drying sensitive samples. E.g. with cantilevers
|
- Drying sensitive samples. E.g. with cantilevers
|
- Drying all kind of samples.
|
| Substrates
|
Batch size
|
|
|
- 1-25 100 mm wafers
- 1-25 150 mm wafers
|
- ? 50 mm wafers
- 1-25 100 mm wafers
- 1-25 150 mm wafers
|
- 1 to 5 wafers per run. Sizes: 2”, 4" or 6"
- Pieces (up to 10x10mm)
|
- 1-25 50 mm wafers
- 1-25 100 mm wafers
- Pieces if a suitable carrier is available
|
- All kind of samples and wafers
|
| Allowed materials
|
|
- Only for RCA cleaned wafers
|
|
|
- Si,SiO2, Si3N4
- Quartz and Pyrex
- InAlP, GaAs
- SU8
|
- No restriction except for polymers
|
|
Choose a drying equipment