Specific Process Knowledge/Thin film deposition/Deposition of Tantalum
Appearance
Feedback to this page: click here
Tantalum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Alcatel) | Sputter (Lesker) | |
|---|---|---|
| General description | E-beam deposition of Ta | Sputter deposition of Ta |
| Pre-clean | RF Ar clean | RF Ar clean |
| Layer thickness | 10Å to 1µm* | 10Å to |
| Deposition rate | 2Å/s to 15Å/s | ~0.3Å/s |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment |
* For thicknesses above 200 nm permission is required.