Jump to content

File:Steamer process develop fig4.png

From LabAdviser
Revision as of 12:27, 29 September 2014 by Paphol (talk | contribs) (Silicon dioxide thickness variation with growth time (from 0 to 720 minutes) in different temperature)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Steamer_process_develop_fig4.png (676 × 502 pixels, file size: 19 KB, MIME type: image/png)

Silicon dioxide thickness variation with growth time (from 0 to 720 minutes) in different temperature

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:27, 29 September 2014Thumbnail for version as of 12:27, 29 September 2014676 × 502 (19 KB)Paphol (talk | contribs)Silicon dioxide thickness variation with growth time (from 0 to 720 minutes) in different temperature

Metadata