Revision as of 12:26, 29 September 2014 by Paphol (talk | contribs) (The percent different of the silicon dioxide thickness at the steamer flow rate at 10 and 25 l/min variation with temperature)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Steamer_process_develop_fig3.png (676 × 502 pixels, file size: 15 KB, MIME type: image/png)

The percent different of the silicon dioxide thickness at the steamer flow rate at 10 and 25 l/min variation with temperature

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:26, 29 September 2014Thumbnail for version as of 12:26, 29 September 2014676 × 502 (15 KB)Paphol (talk | contribs)The percent different of the silicon dioxide thickness at the steamer flow rate at 10 and 25 l/min variation with temperature